Waa maxay foosto mataano ah oo isbarbar socota sideese u shaqeysaa?

2026-07-23 0 Fariin ii dhaaf
<span style="display:none;" id="__kindeditor_bookmark_start_4__"></span>Waa maxay Foostada Isbarbar-dhigga ee Mataanaha? Siday U Shaqeyso | Nanhaiya


A barmiil mataano isku mid ahwaxa uu haystaa laba boolal oo dhexroor joogto ah oo dhinac dhinac ah oo ku jira shaxan-sideed. Boolalku way is-rog-rogmadaan oo waxay hore u riixaan alaabta iyagoo ku dabinaya duullimaadyada dhexdooda, halkii ay ka soo jiidi lahaayeen gidaarka sida hal baalle u sameeyo. Laba doorasho oo naqshadeed ayaa go'aaminaya waxa mashiinku samayn karo: jihada wareega (isku-wareejinta ama rogida) iyo sida qoto dheer ee muraayadaha muraayadaha (si buuxda, qayb, ama aan dhammaan). Hel labadaas mid sax ah oo isku mid ah qalabyada qalabka, hawo-mareenada, ama soo saara PVC adag.

Weydii saddex alaab-qeybiyeyaal waxa barmiil mataano isbar-bar socda ah oo aad ka heli saddex jawaabood oo aan caddayn oo ku saabsan "laba boolal halkii aad mid ka heli lahayd." Taas ayaa hoos u dhigaysa. Habaynta mataanaha ayaa wax ka beddesha sida walxuhu u dhex maro mishiinka, farqigaas farsamo ee keli ah ayaa ah sababta boolal mataano ah ay u qabtaan shaqooyinka hal baalle ma qaban karo.

Hagahan waxa uu daboolayaa makaanikada, labada faas ee kala soocida ee go'aamiya waxqabadka, tafaasiisha alaabta dhabta ah, iyo cabbirka. Si aad u hesho sawirka qaybta ballaadhan, eeg ourextruder furaha foosto hagaha.

Waa maxay Foostada Tooska ah ee Mataanaha Isbarbar-dhiga?

Barmiil mataano ah oo isbarbar socda waa unugga balaastiigga ah ee furaha furaha mataanaha ah. Waxay leedahay laba qaybood oo u shaqeeya sidii hal nidaam: foosto ay ku rakiban yihiin laba dalool oo is-dul-saaran, oo samaynaysa qayb-sideed iskutallaab ah, iyo laba boolal oo dhex fadhiya boolalkaas.

Barbar socdaMacnaheedu waa boolalku waxay ilaalinayaan dhexroor isku mid ah laga bilaabo dhamaadka quudinta ilaa dhamaadka dheecaanka. Caloosha waxay ku sugnaanaysaa isla cabbir dhererkeeda oo dhan. Taasi waa farqiga qeexan ee mataanaha conical, halkaas oo labadooduba boolal iyo boolalba ay hoos ugu dhufanayaan dhinaca dhinta.

Foomka isku midka ah wuxuu siinayaa naqshadeeyaha qayb iskutallaab ah oo joogto ah si uu ula shaqeeyo dhererka oo dhan, taas oo ka dhigaysa mid toos ah in la dhiso mashiinno dhaadheer oo leh qol loogu talagalay isku-dhafka, hawo-qaadista, iyo isku-dhafka qaybaha. Isbarbardhigga u dhexeeya labada foom waxa lagu daboolay annagaconical vs barbar hagaha.

Parallel twin screw barrel set manufactured by Nanhaiya
Furo mataano ah oo isbarbar socda iyo set foosto. Boolalku waxay hayaan dhexroor joogto ah oo ay weheliyaan dhererka shaqada oo dhan.

Sida Foosto Mataanaha Isbarbar yaacaya u Shaqeyso, Talaabo Talaabo ah

  1. Quudinta.Walxuhu waxay ku dhacaan dhuunta quudinta waxayna ku dhacaan labada boolal hal mar. Kaashashka mataanaha ah waxay qaataan budo, jajabyo, iyo quudin aan joogto ahayn taas oo hal furuhu uu ku dhibtoonayo inuu qabsado.
  2. GudbintaBoolalku way jeestaan ​​oo duullimaadka mid kaabku wuxuu tirtiraa kanaalka kale. Alaabtu waxay ku xayiran tahay qolalka qaabka C ee u dhexeeya duullimaadyada waxaana hore loogu sii riixayaa si farsamaysan.
  3. dhalaalayKuleyliyeyaasha foosto ayaa bixiya qeyb ka mid ah kulaylka. Inta soo hartay waxay ka timaadaa dhogorta maaddaama maadada lagu shaqeeyo farqiga cidhiidhiga ah halkaasoo boolaluhu ay isku dhejiyaan, taas oo ah aagga ugu daran ee mashiinka.
  4. Isku qasWareeg kastaa wuu kala baxaa, laalaa, oo dib u celiyaa qulqulka dhalaalka. Kala qaybintaas soo noqnoqota ayaa ah waxa si siman u kala firdhiya buuxinayaasha, midabada, iyo waxyaalaha lagu daro.
  5. Hawo-qaadisFoostada la sii daayay, kanaalka ayaa sii qoto dheereeya dakadda hawo-mareenka markaas cadaadisku wuxuu hoos ugu dhacayaa eber u dhow. Qoyaanka iyo kacsanaanta ayaa halkaas ku baxsada, inta badana madhan.
  6. Bamgareynta iyo cabbiridda.Qaybta ugu dambeysa waxay dhistaa cadaadis waxayna keentaa dhalaal joogto ah dhinta ama pelletizer-ga.
Wax-soo-saarka isku-xidhka mataanaha ee Nanhaiya.

Isku-wareejin vs ka-wareejin: laba jiho, laba shaqo

Boolalku waxay u rogi karaan isla jihada ama jiho ka soo horjeeda. Mid ka mid ah doorashadaas ayaa si buuxda u beddeleysa dabeecadda mashiinka.

Isku-wareejin rogaal celin
Jihada maroodiga Labada boolalba isku si bay u leexdaan Isbuunyadu waxay u leexdaan jihooyin iska soo horjeeda
Jidka alaabta Wuxuu raacaa jaan-siddeed ku wareegsan labada boolal Lagu tuujiyey ibta u dhaxaysa boolalyada
Shear Sare, oo lagu hagaajin karo iyada oo loo marayo walxo isku dhejis ah Hoose, oo si tartiib ah alaabta
Xawaaraha isku dhufashada Sare Hoose
Dhisidda cadaadiska Dhexdhexaad Xoog badan oo deggan
ugu fiican Isku-darka, Masterbatch, Extrusion falcelin, xeryahooda buuxa Dhuumaha PVC ee adag iyo astaanta, walxaha kulaylka-xasaasi ah

Isku-wareejinboolal waa qalabka isku dhafka ah. Xiritaanka sare iyo xawaaraha sare ayaa si fiican u kala firdhiya fiber galaas ah, midab, iyo wax lagu daro, taas oo ah sida saxda ah ee iskudhis la bedelay u baahan yahay.

rogaal celinboolal waxay u dhaqmaan sida bamka barakicinta togan. Neefta udhaxeysa waxay horay u sii qaadaa walxaha cadaadis xoogan oo xiirid hooseeya, taasina waa waxa ay dalbanayaan PVC adag, maadaama PVC ay hoos u dhigto markaad si adag u xiirto. Ourfoosto mataano ah oo isbarbar socda oo isbarbar socdawaxaa loo dhisay waajibkaas, kimisteriga ka dambeeyana wuxuu ku fadhiyaa annagaTilmaamaha foosto caaga ah ee PVC.

Counter-rotating parallel twin screw barrel for PVC extrusion by Nanhaiya
Qalab rogaal celis ah. Neefta u dhaxaysa boolalku waxay hore ugu soo shubtaa xiirid hoose.

Si buuxda, Qayb, ama Aan Meshing ahayn: dhidibka Inta badan Hagayaasha bood

Jihada wareegtadu waa kala badh kaliya ee kala soocida. dhidibka labaad waa sida qoto dheer ee labada boolal ay midba midka kale, oo hagayaasha badankoodu marnaba ma sheegaan.

Kaashashka mataanaha ah ee isku midka ah waxay u kala baxaan saddex nooc:si buuxda u isku-dubbaridisa, qayb ka mid ah meshing, iyo non-meshing. Farqiga u dhexeeyaa waa inta duullimaad ee mid ka mid ahi uu gaadho kanaalka kale.

  • Meshing si buuxdaDuullimaadka mid ka mid ah furku wuxuu gaaraa xididka kan kale, isagoo ka tagaya faraq yar. Kani waa nooca ugu badan ee balaastigga, sababtoo ah nadiifinta cidhiidhiga ah waxay siinaysaa xiirid heer sare ah iyo isku dhafka waxayna tirtirtaa kanaalada nadiif ah marka ay boolalku noqdaan.
  • Qayb ahaan meshingBoolalku way is dulsaaran yihiin, laakiin si qoto dheer bay u yar yihiin. Soo gudbintu waxay ahaanaysaa mid togan marka ay xiiridu soo dhacayso, taas oo ku habboon shay aan qaadan karin shaqo dagaal leh.
  • Aan meshing.Dabaqyadu way dhinac fadhiyaan iyagoon hawlgelin. Mashiinku wuxuu u dhaqmaa in ka dhow laba boolal oo keliya oo ku jira hal foosto, oo leh daaweynta ugu fudud iyo gudbinta ugu wanaagsan.

Qaadashada wax ku oolka ah ayaa ah in "screw twin" keligiis uusan qeexin mashiinka. Isku-dubbarid buuxda iyo is-rog-rogid waa qalab ka duwan kan si buuxda isku-dubbarididda iyo is-beddelka, labaduba waxay ka duwan yihiin habayn aan isku-dubbarid lahayn. Markaad qeexdo qalabka beddelka, nooca meshing waa inuu ku habboon yahay mashiinka aad leedahay.

Waa maxay sababta Twin Screws u gudbiyaan si ka duwan kuwa kali kali ah

Hal baalle waa bamka jiid. Waxay ku tiirsan tahay is-jiidh: walxuhu waa inay ku dhegaan gidaarka foosto in ka badan inta ay ku dheggan yihiin furka, ama waxay si fudud u wareegaan meeshii halkii ay hore u socon lahaayeen.

Ku-tiirsanaantaasi waxay sababtaa dhibaatooyin dhab ah. Budada, jajabka, iyo quudinta sibidhka ama jilicsanaanta hoose si fiican uma qabtaan, sidaas awgeed qashin-qubka ayaa kor u kacaya ama gaajoonaya. Wax-soo-saarka ayaa markaas ku kala duwan sida wanaagsan ee ay u dhacayso in maadada ay qabato maalintaas.

Kaashashka mataanaha ah waxay u gudbiyaan si togan. Duulimaadka hal baalle ayaa xaaqaya kanaalka kan kale, markaa walxo si farsamaysan ayaa loogu riixaa haddii ay qabsato derbiga iyo haddii kale. Wax-soo-saarku waa uu sii socdaa, oo quudinta guuldarradu waxay ku socotaa cabasho la'aan.

Taasi waa sidoo kale sababta boolal mataano ah u xukumaan isku-darka iyo shaqada budada PVC. Isbarbardhigga buuxa ayaa ku jira annagahal furmo vs hagaha furka mataanaha ah.

Waa maxay Foosto Mataanaha Isbarbarya ee Ka Samaysan

Birta salku waxay qaadaysaa culayska farsamada. Dusha sare ee dusheeda waxay qaadataa xirashada. Waa kuwan qeexitaannada aan ku dhisno isku-xidhka isku-xidhka mataanaha ee isku midka ah.

Tilmaamid Qiimaha
Qalabka saldhigga ah 38CrMoAlA
Adag ku daawaynta kulaylka HB260-320
adkaanta nitriding HV950-1000
Moolka nitriding 0.50-0.70 mm
Jajabka nitriding Fasalka 1 ama ka wanaagsan
Dusha oo qallafsan Ra0.4
Marooji toosnaanta 0.015 mm
Adkeydka dahaadhka Chrome HV950 ama ka sareeya
Dhumucda Chrome 0.05-0.10 mm
adkaanta bimetallic HRC60-65
Moolka bimetallic 2.0-3.0 mm

Laba lambar oo shaxdaas ku jira waxay mudan yihiin fiiro gaar ah markaad barbardhigto xigashooyinka.Ku dhaji toosnaanta 0.015 mmWuxuu go'aamiyaa bal in boolalku run yihiin shaxan-sideed, furka qaloocsan wuxuu xidhaa dhinac ka mid ah boodhka oo wuxuu baabi'iyaa beddelkiisa sidoo kale.Jajabka nitridingwaa hubinta tayada badi alaab-qeybiyeyaasha weligood ma daabici karaan: kiis adag oo jajaban oo ka jaban culeyska hoostiisa halkii ay iska caabin lahaayeen xirashada.

Marka laga soo tago dhismaha caadiga ah, waxaan u habeyneynaa birta shaqada kulul, birta shaqada qabow, birta xawaaraha sare leh, birta budada HIP, iyo Alloys PTA. Marka quudintu noqoto mid xoqan ama daxalaysa, dariiqa bimetallic ayaa beddelaya nitriding, iyo annagabimetallic vs nitrided guidedaboolaya marka ay taasi bixiso.

Cabbirka: Dhexroorka, L/D, iyo wax soo saarka

Dhexroorka maroojinta ayaa dejinaya wax soo saarka L/D ayaa dejisa inta qol ee mishiinku leeyahay si uu u dhalaaliyo, u qaso, oo uu u soo daayo inta uu socdo. Waa kuwan moodooyinka isku midka ah ee mataanaha ah ee sida caadiga ah loo isticmaalo oo leh tirooyinka wax soo saarka ee PVC.

Qaabka Dheecaan maroojin (mm) L/D Wax soo saarka PVC (kg/saacaddii) Xawaaraha wareegtada (rpm) Matoorka (kW)
NHY75 75 26–36 220-350 45 45
NHY90 90 26–36 280-460 45 55
NHY110 110 26–36 350-650 45 75
NHY120 120 26–36 500-800 45 110
NHY130 130 26–36 680-1000 45 132

Akhri qaabka halkii aad ka heli lahayd kaliya safafka. Wax soo saarku wuxuu si qiyaas ah u eegayaa dhexroorka, korantada matoorkana way la fuulaysaa, sababtoo ah ku riixida walxo badan waxay qaadanaysaa wareeg badan. Kooxda L/D waxay ahaanaysaa isku mid marka loo eego kala duwanaanta, maadaama saamigu yahay doorashada naqshadaynta halkii ay ka ahaan lahayd natiijada cabbirka.

Moodooyinkan bannaanka waxaan ka dhisnaa biro is barbar socda laga bilaabo 45 mm ilaa 150 mm, iyadoo L/D laga bilaabo 32:1 ilaa 38:1 ay ku jirto tuubooyinkayada PVC-ga ama ku habboon khadkaaga. Waxa L/D dhab ahaan ku soo gadayo waxa lagu daboolay hagaha saamiga L/D, kala duwanaanshana waxay ku fadhidaa annagabar-barro mataano ah bogga sheyga.

Hal qoraal oo ku saabsan tirooyinka wax soo saarka:nambarada kg/h ee kore waxaa loogu talagalay PVC. Beddel polymerka, habaynta, ama dhinta, oo wax-soo-saarka ayaa la socdaa. Ula dhaqan wax soo saarka la daabacay sidii tixraac cabbir cabbireed, ka dibna ka xaqiiji sidaad u qaadan lahayd.

Waa maxay Isbarbardhigga Mataanaha Isku-dhafka ah ee Dhab ahaantii Soo saara

Afar qoys oo codsade ah ayaa daboola inta badan waxa mishiinadani qabtaan, waxayna ka soo bilowdaan alaabta ceeriin ilaa badeecada dhammaatay.

Wax ka beddelka caagagga iyo isku-darka

Codsiga ugu caadiga ah. xiirid xooggan iyo awood kala firdhis waxay u oggolaanaysaa polymer-ka aasaasiga ah sida PP, PE, ama ABS in si siman loogu walaaqo fiber galaas, fiber carbon, dab-dejinta, iyo antioxidants. Taasi waxay soo saartaa darajooyin la xoojiyay, olol-dejiya, ama korantada, sida PP-ga lagu xoojiyay galaas-fibre-ga ee loo isticmaalo qaybaha baabuurta iyo ololka-dib ABS ee loo isticmaalo elektiroonigga.

Midabka iyo masterbatch shaqaynaysa

Midabka-fiirsashada sare leh, midabaynta, ama wax-ka-qabsiga wax-qabadka ayaa lagu qasaa xabagta side, ka dibna la sii daayay oo la diiray. Tani waxay soo saartaa masterbatch midabka midabaynta, ama masterbatch shaqaynaysa sida darajooyinka antistatic iyo bakteeriyada. Furayaasha mataanaha ah waxay xalliyaan dhibaatada isku dhafka aan sinnayn ee xaddidaysa hal boolal ee shaqadan.

Granulation parallel twin screw for compounding by Nanhaiya
A granulation isbarbar galka mataanaha. Isku-darka iyo pelletizing waxay ku tiirsan yihiin kala-goynta soo noqnoqda iyo dib-u-habaynta dhalaalka.

Qaabaynta dibadda

Dhuumaha, profile, xaashida, iyo filimka. Kaashashka mataanaha ah waxay ku habboon yihiin viscosity-sare, oo ay adag tahay in la-caasiyeeyo polymers sida PVC iyo PC gaar ahaan si fiican. Dhuumaha dheecaanka PVC, albaabka iyo astaanta daaqada, iyo xaashida kombuyuutarku waxay dhammaan ku xidhan yihiin balaastiga labbiska ah ee furka mataanaha ahi keeno, kaas oo ah waxa hoos u dhigaya cilladaha alaabta. OurTuubooyinka PVC ee barmilada isku midka ahu adeegi biyaha iyo dhuumaha dareeraha, marinka korantada, iyo tuubooyinka ilaalinta.

Habaynta balaastiig dib loo warshadeeyay

Qashinka PP iyo PE waxay dhex maraan xiirid iyo kuleyl ka saaraya wasakhda, yaraynaysaa walbahaarka, oo dib u balaastiijiya walxaha pelleting. Quudinta dib loo warshadeeyay waa mid aan iswaafaqsanayn oo inta badan wasakhaysan, taas oo ah nooca saxda ah ee agabka gudbinta wanaagsani si fiican u qabato. 

Sida loo Oggo Marka Isku-bar-bar yaaca Twin Screw Set uu u Baahan Yahay Beddelka

Dharka iskuxiran ee mataanaha ah ayaa ka soo baxa meelo isku mid ah mar kasta, mashiinku wuxuu kuu sheegayaa ka hor intaanay qaybaha u muuqan mid xun.

  • Wax soo saarka ayaa dhacayaxawaare isku mid ah. Nadiifinta da'da ah waxay u oggolaanaysaa dhalaalidda dib u dhac halkii hore loogu socon lahaa.
  • Isku-darka dhibcaha tayada.Xariijimaha midabka ama qaybinta buuxinta aan sinnayn waxay la macno tahay in boolalku aanay si fiican isu masaxayn.
  • Culayska baabuurka ayaa fuulawax soo saar joogto ah, kaas oo tilmaamaya jiidid, is-hagaajin, ama iska caabin wax dhisme oo hoos u dhacay.
  • Meesha tayada korkaon alaabta la dhammeeyey, inta badan waxa ugu horreeya ee waaxda tayada ogeysiiso.

Ku xaqiiji qalabka halkii aad ka arki lahayd. Cabbir duulimaadka OD iyo aqoonsiga dhalada ee ka soo horjeeda sawirka dhismaha, oo hubi nadiifinta intermesh, kaas oo u gaar ah boolal mataano ah oo fudud in la iska indho tiro. 

Kaashashka mataanaha ah waa lammaane isbarbar socda.Nadiifinta intermesh-ka ayaa la dejiyay inta lagu jiro wax soo saarka. Beddelidda furaha iyo ilaalinta kan kale soo celin mayso nadiifintaas, waana sababta loo soo saaro boolal mataano ah, la keeno, loona beddelo laba-labo.

Maxaad ula shaqeysaa Nanhaiya

Nanhaiya waxay dhistay boolal iyo fuustooyin in ka badan labaatan sano waxayna u adeegtaa 500+ macaamiisha adduunka oo dhan. Ourkala duwan oo ah boolal mataano isbarbar socdadaboolaya isku-darka, granulation, PS xumbo, guddi aluminium-cag ah, caag iyo balaastig ah, iyo waajibaadka tuubada PVC, ee isku-wareeg iyo isku-rogid qaabeynta.

Qayb kasta waxaa laga farsameeyay 38CrMoAlA waxaana lagu dhammeeyay tafatirka shaxda sare, iyadoo leh kontorool dulqaad adag iyo tijaabin dheellitiran oo firfircoon ka hor intaysan dhoofin. Qalabyadayada waxaa loo dhisay si ay ugu habboonaadaan noocyada waaweyn ee wax-ka-baxa oo ay ku jiraan KraussMaffei, Cincinnati, iyo Jwell, waxaanan ku habeyneynaa astaanta furaha, saamiga isku-buufinta, naqshadeynta hawada, iyo aagagga kuleylinta khadkaaga.

Kahor intaadan soo xigan, injineeradayadu waxay kula shaqeeyaan halbeegyada: dhexroorka, saamiga dhinaca, qoto dheer ee jeexjeexa jeexdin, iyo xulashada walxaha. Xigashadani waxay dabooshaa alaabta, rarida, iyo kharashka dayactirka ee la filayo, waxayna kugu soo gaadhaysaa 12 saacadood gudahood. Bixinta kadib, farsamayaqaanadeena waxay taageeraan rakibaadda iyo hawlgelinta, iyo arrimaha iibka kadib waxay helaan jawaab 24 saacadood gudahood.

Ma u baahan tahay isku-xidhka mataanaha ah ee isku midka ah ee lagu dhisay mashiinkaaga? Soo dir moodeelkaaga, sawir ama muunad xidhan, oo lagu daray alaabta aad wado. Waxaan soo xiganeynaa 12 saacadood gudahood.

Hel Xigasho Twin Screw

Su'aalaha Inta Badan La Isweydiiyo

Waa maxay barmiil mataano ah oo isbarbar socda?

Waa unugga balaastiigga ah ee fidiyaha furayaasha mataanaha ah: foosto leh laba boos oo is dulsaaran oo samaynaysa qayb-sideed iskutallaab ah, oo haysata laba boolal dhexroor joogto ah. Kaashashka ayaa si farsamaysan u gudbiya agabka iyagoo ku dabinaaya duulimaadyadooda dhexdooda, halkii ay ku tiirsanaan lahaayeen khilaaf ka soo horjeeda gidaarka foosto.

Sidee buu u shaqeeyaa barmiil mataan ah oo isbarbar socda?

Walxuhu waxay ku dhacaan labada boolal ee cunaha quudinta. Sida boolaluhu u jeestaan, duullimaadka mid ka mid ah ayaa tirtiraya kanaalka kan kale, isagoo dabinaya walxaha oo u sii riixaya hore. Kuleyliyeyaasha foostada iyo dhogorta aagga isku dhafka ah way dhalaalaan, wareeg kastaa wuu kala baxaa oo dib u soo celiyaa dhalaalka si uu u qaso, iyo qaybta ugu dambeysa waxay dhistaa cadaadis si ay u quudiso dhimashada.

Waa maxay farqiga u dhexeeya isku-wareejin iyo wareeg-wareejin?

Iskoollada iswada-wareegaya waxay u leexdaan si la mid ah waxayna keenaan xiirid sare xawaare sare, kaas oo ku habboon isku-darka, masterbatch, iyo xeryahooda buuxa. Iskoolada rogaal celiska ah waxay u leexdaan jihooyin iska soo horjeeda waxayna u dhaqmaan sida bamka barakicinta togan, iyagoo ku dhisaya cadaadis xoog leh xiirid hoose. Ficilkaas fudud ayaa ah waxa tuubbada PVC ee adag iyo baahida profile.

Maxay yihiin kuwa si buuxda isku-dubbaridaya, qayb-ka-dhafan, iyo furayaasha mataanaha ah ee aan is-daba-marin?

Waxay sharxayaan sida qoto dheer ee labada boolal ay isula jiraan. Naqshado si buuxda loo xidho ayaa xididka midba midka kale ku leeyahay farqi yar, isagoo siinaya xiirid iyo isku dhafka ugu fiican, tanina waa nooca ugu badan ee balaastigga. Qaybaha isku-xidhka-xidhka ah way yareeyaan oo waxay yareeyaan xiirta. Iskoolada aan is-daba-joogga ahayn waxay u fadhiyaan dhinac-dhinac iyagoon mashquulin, iyagoo siinaya daaweynta ugu fudud.

Waa maxay farqiga u dhexeeya boolal mataano ah oo isbarbar socda iyo kuwa koonka ah?

Kaashashka mataanaha ah ee isku midka ah ayaa ilaaliya dhexroor isku mid ah laga bilaabo quudinta ilaa dareeraha, iyo boodhku wuxuu ahaanayaa cabbir joogto ah. Tapers mataano toniile ah, oo leh dhamaadka quudinta ka weyn oo ku soo cidhiidhiday dhinaca dhinta. Foomka isku midka ah wuxuu siinayaa qaybta isdhaafka ah ee joogtada ah ee dhererka, taas oo ka dhigaysa mashiinno dhaadheer oo leh qaybo hawo-qaadis iyo isku-dar ah oo toos ah si loo dhiso.

Maxaad u isticmaashaa furaha mataanaha ah halkii aad ka isticmaali lahayd hal fur?

gudbinta togan Hal furuurtu waxay ku tiirsan tahay is-jiidhid, sidaa darteed shayku waa inuu qabsado gidaarka foosto si ay hore ugu socdaan, budo, jajabyo, iyo quudin sibiq leh ayaa keena kor u kaca. Kaashallada mataanaha ah waxay si farsamaysan u riixaan walxo iyadoon loo eegin xajin, taasoo siinaysa wax-soo-saar joogto ah oo u ogolaanaya inay xakameeyaan quudinta ka adkaata hal mar.

Maxaa isbar-bar yaaca mataanaha loo isticmaalo?

Afar qoys oo waaweyn: wax ka beddelka caagga ah iyo isku-darka fibre dhalo, kaarboon-fibre, ama dab-celiyayaal; midabka iyo wax soo saarka masterbatch functional; soo saarista tuubooyinka, profile, xaashida, iyo filimada oo ay ku jiraan PVC iyo PC; iyo warshadaynta balaastiig ah oo dib loo warshadeeyay halka qashinka PP iyo PE lagu nadiifiyo, dib loo caageeyay, lagana nadiifiyo.

Furayaasha mataanaha ah ma in loo beddelaa lammaane ahaan?

Haa Nadiifinta intermesh ee u dhaxaysa labada boolal waxa la dejiyay inta lagu jiro warshadaynta oo laguma soo celin karo iyada oo lagu beddelayo hal bir oo ka soo horjeeda lammaane xiran. Furayaasha mataanaha ah ayaa la soo saaraa, la keenaa, oo loo beddelaa sidii lammaane is-bar-bar socda, waana in la kaydiyaa oo sidaas loo qabtaa.

Wararka la xidhiidha
Fariin ii dhaaf
X