Keli vs Twin Screw Pelletizing Line | Hagaha Iibsada

Xariiqda saxda ah laguma go'aamiyo tirinta biraha oo keliya. Waxaa lagu go'aamiyaa waxa ay tahay in ay ka dhacaan inta u dhexeysa xoolo aan sinnayn iyo pellet la aqbali karo: quudi, dhalaalin, qas, ka saar gaaska, shaandhaynta wasakhda, cadaadis dhis, gooyo oo qalaji.

Nanhaiya single-screw pelletizing machine Nanhaiya parallel twin-screw pelletizing machine
Xariiq hal-baro ah ayaa ah dariiqa tooska ah ee waajibaadka dhalaalidda iyo dhalidda deggan. Khadka mataanaha ah ee isku midka ah wuxuu kasbadaa kakanaanta dheeraadka ah marka la isku daro, kala firdhiyo, quudin heersare ah ama gooni-u-goontu ay keento tayada alaabta.

Dooro axariiqa pelletizing ee hal-dharoolemarka xooluhu ay mar horeba ku dhow yihiin qaabaynta u dambaysa iyo shaqooyinka ugu waaweyni waa gudbinta xasiloon, dhalaalidda, dhalaalidda sifaynta, abuurista cadaadiska iyo goynta pellet. Waa meel bilow ah oo wax ku ool ah oo loogu talagalay dib-u-kicinta PE ama PP ee joogtada ah, dib-u-kicinta fudud, shaqada shaybaadhka iyo wax-soo-saarka yar iyo midka dhexe.

Dooro akhadka pelletizing ee mataanaha ah ee barbar socdamarka mishiinku waa inuu isku daraa iyo sidoo kale pelletize. Way ku habboon tahay buuxinta, midabada, isku-darka polymerka, masterbatch, balaastikada la beddelay, durdurrada quudinta badan iyo gooni-gooni xoog leh. Ha iibsan khadka mataanaha ah sababtoo ah wax soo saarkiisa liiska ayaa sarreeya. Iibso marka hawsheeda hab-socodkeedu ay ku habboon yihiin qaabaynta.

Ka bilow isbeddelka walxaha, ma aha magaca mashiinka

Iibsaduhu wuxuu inta badan na weydiiyaa khad mataano ah ka dib markuu arko ereyada "wax soo saarka sare" ama "isku darka ka wanaagsan." Taasi waxay ka booddaa su'aasha ugu muhiimsan: waxa soo galaya hopper, iyo sidee bay u kala duwan tahay ka hor intaysan gaarin bacda?

Haddi ay nadiif yihiin, granulles lebbisan kaliya waxay u baahan yihiin in la dhalaaliyo oo mar kale la gooyo, mashiinka isku dhafan ee isku dhafan ayaa ku daraya kontaroolada, nadiifinta shaqada iyo xidhashada dhibcaha iyada oo aan daruuri ahayn hagaajinta pellet la iibin karo. Haddii dhowr budo, midabeeyayaal iyo polymers ay noqdaan hal unug oo joogto ah, fur fudud oo gudbinta ayaa laga yaabaa inay ka tagto dhibaatada tayada dhabta ah ee aan la taaban.

Waajibka wax soo saarka Meesha ugu fiican ee laga bilaabo Waa maxay sababta Maxaa bedeli kara jawaabta
Dib-u-kicinta qulqulka PE ama PP deggan, la soocay Kaashashka kali ah Dhalitaan toos ah, abuurista cadaadiska iyo sifaynta leh kakanaanta khadka hoose Qoyaanka, ur, daabacaadda, qulqulka dhalaalka isku dhafan, waxyaabaha lagu daro ama wasakhda culus
Filimada dib loo warshadeeyay ee cufnaanta cufnaanta hoose leh Keli ah oo leh quudin la farsameeyay Dhalada koowaad waxay noqon kartaa joogteynta quudinta, ma aha isku darka Qalalaasaha daran, polymers-ka isku dhafan ama hagaajinta cuntada ayaa laga yaabaa inay door bidaan furayaasha mataanaha ah
Midabka ama wax lagu daro masterbatch Isbarbar yaaca mataanaha Walxaha isku dhafka ah ee moodeelka ah iyo walaxda la xakameynayo ee kordhinta waxay taageertaa fidinta Cunto la hubiyay oo la isku daray oo leh baahi firidhsan oo dhexdhexaad ah ayaa laga yaabaa inay ku shaqeyso fur keliya oo khaas ah
Kaalshiyam carbonate ama iskudhis kale oo buuxa Isbarbar yaaca mataanaha Quudinta goonida ah iyo aagagga kala firdhisan ee la habayn karo Soo-buuxinta buuxinta, foomka qayb ka mid ah, xoqidda iyo isku-duubnaanta hantida loo baahan yahay
Polymer alloy ama wax ka beddelka falcelinta Isbarbar yaaca mataanaha Deganaanshaha, isku darka iyo hawo-qaadista waxaa lagu habayn karaa iyadoo la raacayo aagga habraaca Kinetics falcelinta, dareenka kulaylka iyo baahida cadaadiska hoose
Shaybaadhka ama pilot dib-u-pelleting Kaashashka kali ah Qaabaynta is haysta, hawl fudud iyo dayactir fudud Tijaabada lafteeda waxa laga yaabaa inay u baahato isku xidhid modular dabacsan
Dhismaha PVC Qeex cunto karinta marka hore Labada qoys ee khadka Nanhaiya waxay taxayaan PVC, laakiin waxay u adeegaan hawlo kala duwan Quudinta budada, dareenka kulaylka, buuxinta, balaastiga, isku dhafka iyo habka goynta pellet
Balaastii hore ee wax laga beddelay Isbarbar yaaca mataanaha Awoodda xariiqda daabacan ee sare oo ay weheliso isku-dhafka, quudinta dhinac-quudinta iyo ikhtiyaarrada gooni-goonida Ha ku cabbirin kg/saac oo keliya; torque, cufnaanta bulk iyo qeexida alaabta ayaa dejisay heerka la isticmaali karo

Aragtida warshadeena:mashiinka ugu jaban waa xariiqda dhamaystiraysa isbeddelka loo baahan yahay iyada oo aan lagu darin marxalado aan loo baahnayn. Mararka qaarkood taasi waa halbeegga kaliya. Mararka qaarkood furka mataanaha ah wuxuu ka hortagaa isku-darka soo noqnoqda, labajibbaaran oo dibadda ah ama pellets-ka-baxsan. Waxaan ka door bidi lahayn inaan aragno cunto karinta buuxda halkii aan ka ahayn tirinta furaha la doortay ee iibsadaha.

Xariiqda pelletizing waa silsilad heerar habraac isku xidhan

Labada noocba waxay u baahan yihiin wax ka badan duuliye. Nanhaiya'skala duwan ee mashiinka extruder caag ahwuxuu qeexayaa shan nidaam oo xudun u ah: quudinta; balaastiig leh fur, foosto, kululaynta iyo qaboojinta; gudbinta; madaxa dhiman; iyo qaabaynta, qaboojinta iyo jiidashada. Mashruuca pelletizing, shaandhaynta, jarista, qalajinta ama baadhista iyo ururinta dhamaystirka silsiladda.

1. Diyaari oo quudi

Qeex in galinta ay tahay pellet, budo, jajab, filim, agglomerate ama isku darka. Cufnaanta badan, isku xidhka iyo xasilloonida heerka quudka ayaa go'aamiya in loo baahan yahay quudiye cufisjiid, quudiye qasab ah ama quudiyeyaal miisaan lumis ah oo kala duwan.

2. dhalaali oo beddel

Furaha iyo foosto waa inay dhalaaliyaan, gudbisaa oo ay isku daraan iyada oo aan ka badnayn heerkulka walxaha ama xadka xiirid. Isku-darka, khadka ayaa sidoo kale u baahan kara quudin dhinaca, qaybaha cajiinka iyo hawada hawada ama faakuumka.

3. Shaandhee oo dhis cadaadiska

Beddelaha shaashadu waxa uu ka saaraa wasakhowga jidhka ee aan dhalaalin. Dhimashadu waxay u baahan tahay cadaadis iyo qulqul joogto ah, markaa dareeraha furka, ikhtiyaarka bamka dhalaalay iyo aagga sifaynta waa in loo cabbiraa hal qayb.

4. jar dhalaalka

Strand, giraanta biyaha iyo nidaamyada biyaha hoostooda waxay u abuuraan pellets siyaabo kala duwan. Qulqulka xoogga, dhegdhegnaanta, dareenka biyaha, wax soo saarka iyo isbeddelka joogtada ah waa arrin ka badan caadada.

5. Qabow, qallaji oo kala saar

Heerkulka biyaha, wakhtiga la deggan yahay, biyo-baxa iyo baadhistu waxay saameeyaan heerkulka pellet, qoyaanka, ganaaxyada iyo qaabka kaydinta ka hor.

6. Xakamee khadka

Aagagga heerkulka, xawaaraha, ilaalinta matoorka, cadaadiska, heerka quudiyaha, faakuumka iyo qaylo-dhaanta waa inay u sheegaan hawlwadeenka haddii marxalad kastaa ay deggan tahay. Bandhiga kaligiis ma sameeyo habka la xakameeyo.

Complete Nanhaiya single-screw pelletizing line with cooling and collection equipment
Xigasho dhamaystiran waa in ay tilmaamto marxalad kasta laga bilaabo quudiyaha ilaa ururinta pellet. Haddii kale, laba alaab-qeybiyeyaal ayaa laga yaabaa inay isticmaalaan magac isku mid ah oo kala duwan.

Marka xariiqa pelleting-ka-kaliya uu ku filan yahay

A extruder-kaliyawuxuu asal ahaan ku xoogan yahay gudbinta joogtada ah, dhalaalka iyo abuurista cadaadiska. Waxa kale oo ay bixin kartaa isku darka qaybinta faa'iido leh marka joomatari screw, mixer iyo barta qalliin ay ku habboon yihiin walxaha. Taasi waxay ka dhigaysaa saldhig macquul ah oo dib-u-fududeynta kaydka quudinta ee mar hore la soocay, la isku daray ama la habeeyey.

Xariiqda pelletizing-ka-kaliya ee Nanhaiya waxa uu isku daraa faashad-fure, dhalaali sifaynta, madaxa dhinta, qaboojinta biyaha, pelletizer iyo unugga ururinta. Codsiyada liiska ku jira waxaa ka mid ah bikrad ama balaastiig dib loo warshadeeyay, shaybaarro, wax soo saar tijaabo ah iyo pellets oo loogu talagalay qaabeynta duritaanka, afuufista filimada ama extrusion. Ikhtiyaarka ikhtiyaariga ah ee beddelka shaashadda, faakuum-dejinta iyo quudinta kaalmaynta waxay u oggolaanaysaa khadka aasaasiga ah inuu maareeyo xaaladaha quudinta ee adag iyada oo aan loo rogin madal isku-dar ah oo buuxda.

Isticmaal hal baalle sida gunta gundhigga marka:Cuntada quudinta ayaa go'an ka hor inta aan la saarin; qoyska polymer-ka iyo dabeecadda dhalaali waa mid joogto ah; kala firdhisan ma aha sheegashada alaabta ugu weyn; faddaraynta waxaa lagu maarayn karaa filtarka la cayimay; Ka saarista aan xasilloonayn waa dhexdhexaad; iyo wax soo saarka waa la hayn karaa iyada oo aan la qasbin quudin aan degganayn ama heerkulka dhalaalidda xad-dhaafka ah.

Nanhaiya single-screw recycling pelletizing line installed in a workshop
Cufnaanta hoose ee dib loo warshadeeyay waxay ka dhigi kartaa qaybta quudinta xadka wax soo saarka dhabta ah. Sheeg foomka quudinta iyo cufnaanta bulk ka hor inta aanad dooran dhexroorka furaha.
Drive and die-side equipment on a Nanhaiya single-screw pelletizing line
Wadista, furka iyo cadaadiska dhinaca dhinta waa in la is waafajiyaa. Qiimaynta mootada lafteedu ma caddaynayso wax soo saarka xasilloon.

Kaashashka kelida ah macnaheedu maaha "ingineeriye ma jiro." Thedesign fur furka granulationweli waxay ku beddeshaa quudinta jajabka, dhererka dhalaalka, booska hawo-mareenka, iska caabinta shaashadda iyo habka pelletizing. Khadku wuxuu yeelan karaa koronto ku filan oo rakiban oo weli kor u kacaysa sababtoo ah hopper wuxuu keenaa walxaha si aan sinnayn ama furku wuxuu lumiyaa shaabadiisa dhalaalaysa ee u dhow hawo-mareenka.

Marka khadka mataanaha ah ee isku midka ah uu helo kharashkiisa dheeraadka ah

Khadka mataanaha ah ee isku midka ah ayaa noqda mid qiimo leh marka extrusion ay tahay in la beddelo qaabka, ee maaha kaliya in dib loo qaabeeyo. Xariiqda Nanhaiya waxay isticmaashaa koronto-dheer oo isbarbar socda twin-screw extruder oo leh walxo fur furan. Nidaamkeeda baaxadda leh waxaa ka mid ah isku darka iyo kala firdhinta waxyaabaha lagu daro, buuxinyaasha iyo midabeeyayaasha, oo lagu daray quudin mataano ah oo ikhtiyaari ah, faakuum-dejinta iyo beddelka shaashadda tooska ah.

Foostada moodada ah iyo tareenka furka ayaa u oggolaanaya naqshaduhu inay ku meeleeyaan shaqooyin kala duwan oo ay weheliyaan mashiinka: gudbin quudin, dhalaaliso polymerka, ku dar buuxinta biyaha hoose, codso shaqo qaybin ama kala firdhisan, u fur dusha dhalaalka si ay u go'do, dhisto shaabad dhalaalaysa oo dejiso dheecaanka. Cilmi-baadhis ku saabsan soo-baxa mataanaha-screw-ka sidoo kale waxay ku xidhaa joomatari dhalaalid degdeg ah iyo isku-dar la wanaajiyey, halka tixraacyada isku-darka warshadaha ay habeeyaan gudbinta, balaastiigga, isku-dhafka, nadiifinta iyo xoojinta cadaadiska sidii aagag hab-socodka oo gooni ah.

Isticmaal fur mataano isbar-bar socda sida gundhigga marka:dhowr maaddo waa in si gooni ah loo cabbiraa; midabka ama buuxinta kala firdhinta waxay xakameysaa qiimaha; qaadashada budada waa adag tahay; habayntu waxay u baahan tahay hal ama in ka badan oo marxalado hawo-qaadis ah; isbeddelka alaabtu waxay u baahan yihiin cunto karis ah fur-fure; ama xariiqdu waa in ay isku xirto oo ay ku dhufataa hal baas oo la kantaroolo.

Nanhaiya parallel twin-screw pelletizing extruder with hydraulic equipment
Extruder-ku waa kaliya qaybta habka dhexe. Quudinta, dareeraha ama budada ku darista, hawo-mareenka iyo qalabka hoose ayaa go'aamiya in awoodeeda isku-darka la isticmaali karo iyo in kale.
Pair of modular parallel twin-screw elements manufactured by Nanhaiya
Qaybaha furaha modulka ah waxay u oggolaanayaan gudbinta iyo isku dhafka hawlaha in lagu habeeyo habaynta. Isku xigxiga walxaha, nadiifinta iyo biraha waxay ka tirsan yihiin sawirka farsamada ee la ansixiyay.

Aragtida warshadeena:Iibka mataanaha ah wuxuu guuldarraystaa goor hore marka alaab-qeybiyaha uu helo kaliya magaca resin iyo bartilmaameedka kg/saacaddii. "PP plus filler" ma aha qeexid habraac. Waxaan u baahanahay boqolleyda buuxinta, qaabka walxaha, cufnaanta bulk, qoyaanka, abrasiveness, qorshaha quudiyaha, bartilmaameedka kala firdhisanaanta iyo heerkulka dhalaalka la oggol yahay. Faahfaahintaasi waxay go'aamiyaan walxaha iyo qaybaha foosto ee iibsaduhu dhab ahaantii ku bixinayo.

Waxyaabaha dib loo warshadeeyay, kala saar afar dhibaato

Weydiimaha dib-u-warshadaynta inta badan waxay isku daraan xasillooni-darrida quudinta, qoyaanka, wasakhda iyo isku-dhafka liita ee hal calaamad: "Wax dib loo warshadeeyey." Dhibaato kastaa waxay u baahan tahay sifada xariiqa ka duwan. Kordhinta xawaaraha iswiidhishka ma hagaajin karo dhamaantood.

Dhibaatada la arkay Su'aasha habsocod ayay u badan tahay Tilmaamaha khadka si loo cayimo Cadeymaha aqbalida
Wax soo saarka ayaa kor u kaca oo dhaca Cufnaanta hoose miyaa isku xidha mise si aan sinnayn baa u quudinaysa? Quudinta khasabka ah, kicinta ama cufnaanta, joomatari hopper deggan iyo xakamaynta quudiyaha Dhaqdhaqaaqa soo-saarka iyo culeyska matoorka ee socodka joogtada ah ee la qeexay
Xumbo, ur ama pellets dalool leh Waa maxay qoyaanka iyo culeyska kacsan ee gala dhalaalka? Qallajinta meesha ku habboon, meesha hawo-mareenka, dhalaalidda shaabadihii, awoodda faakuumka iyo cusboonaysiinta dusha sare Qoyaanka ama natiijada kacsan iyo xadka pellet muuqaal ah
Cadaadisku wuu sii kordhayaa Immisa wasakhaysan oo aan dhalaalin ayaa gaadhay shaandhada? Aagga shaandhaynta, isku xigxiga mesh, nooca wax beddelka shaashadda, dareemayaasha cadaadiska iyo muddada beddelka Cadaadiska kor u kaca iyo isbeddelka shaashadda ee soo-saarka bartilmaameedka
Midabka ama sifooyinka ayaa kala duwan Halabuurka quudinta miyuu is beddelayaa, mise isku-darku kuma filna? Kala soocida sare iyo isku darka marka hore; isku-darka mataanaha ah haddii la rabo in la saxo ama la kala firdhiyo Midabka lagu heshiiyey, dhalaalka-socodka ama kala duwanaanta hantida makaanikada

Ururka dib-u-warshadaynta caaggu waxa uu qeexayaa sifaynta dhalaalka sida ku qasbida balaastiig dhalaalaysa iyada oo loo marayo shaashad fiican si looga saaro biraha, alwaaxyada, warqadaha, heerkulbeegyada iyo wasakhda jirka kale ee aan dhalaalin. Sifeynta kama saari karto polymer kasta oo milmay, ur ama kacsan. Waxa kale oo ay ku darsataa caabbinta socodka, markaa xirmada shaashadda, aagga sifaynta, cadaadiska dheecaanka iyo habka isbeddelka waa in si wadajir ah loo qeexaa.

Mixed colored plastic regrind before pelletizing
Midabka isku dhafan ee quudinta ayaa muuqda. Kiimikada polymer-ka ee isku qasan ayaa laga yaabaa inaysan ahaan. Kala soocida iyo aqoonsiga alaabta ayaa ah kontaroolada tayada sare.
Uniform white plastic pellets after compounding and pelletizing
Pellets u eg lebbiska ma aha heerka aqbalida oo dhammaystiran. Ku dar qoyaanka, ganaaxyada, cufnaanta bulk, qulqulka dhalaalka, midabka ama tijaabooyinka farsamada ee ku habboon isticmaalka hoose.

Dooro habka pelletizing sida qayb ka mid ah khadka

Xulashada sharoobada waxay helaysaa dareenka intiisa badan, laakiin goynta aan xasilloonayn waxay ka dhigi kartaa dhalaal si fiican u caagaysan oo aan la iibin. Xariiqda kaliya ee Nanhaiya waxaa ka mid ah qaboojinta biyaha iyo qalabka wax lagu kariyo. Qadka mataanaha ah ee isku midka ah wuxuu isticmaali karaa giraanta biyaha ama pelletizer strand waxaana ku jira qaboojinta, baarista iyo qaybaha ururinta.

Habka Habka Bar bilow wanaagsan Su'aalaha ka hor intaadan dalban
Xarig biyo-qubeedka Xadhkaha ka saar, ku qabooji weel, ka saar biyaha korka, jiid oo jar Isku-darka dabacsan iyo shaqada dib-u-warshadaynta halkaasoo hawl-wadeenadu ay maamuli karaan xargaha bilowga Dhallaanku ma leeyahay xoog ku filan oo xadhig ah? Immisa jeer ayaa midabku isbeddelaa? Sidee loo maarayn doonaa xadhig jaban?
Xarig qallalan oo la jarjaray ama suunka qaboojiyay Ku qaado xadhkaha kulul suunka hawo, biyo ama qaboojin la isku daray ka hor inta aanad jarin Hababka biyaha xasaasiga ah, jilicsan, laastikada ama aadka loo buuxiyey Dhererka suunka ee loo baahan yahay, culeyska qaboojinta, xawaaraha xadhigga, jajabnaanta iyo bannaanka sagxadda
Weji-gacan-biyoodka Iska yaree wejiga dhiman oo ku qaado pellets giraanta biyaha wareegeysa Isku-dhafan, pelleting joogto ah marka dhalaalku si nadiif ah u gooyo geeridu Baraf-dhimista, daab daab, heerkulka biyaha, qaabka pellet-ka iyo biyo-baxa
Biyaha hoostooda Iska yaree wejiga dhinta gudaha qol biyo ka buuxaan, ka dibna biyo-mareen oo qallaji Hawlgalka otomaatiga ah iyo waajibaadyada pelleting warshadaha ballaaran Heerka ugu yar ee deggan, qashinka bilawga ah, kuleylinta saxanka, nidaamka biyaha, qalajiyaha iyo nadiifinta

Nidaamyada suunka qallalan ee MAAG waxaa loogu talagalay in biyaha xasaasiga ah, aadka loo buuxiyo ama jilicsan, halka nidaamyada biyaha hoostooda ay daboolaan xeryahooda, masterbatch, dib-u-warshadaynta iyo polymers bikradaha. Taasi kama dhigayso hal hab oo caalami ah. Waxay tusinaysaa sababta dabeecadda walaxda dhimashada ka dib ay tahay inay qayb ka noqoto go'aanka iibka.

Multiple polymer strands passing through a Nanhaiya water cooling trough
Xadhkaha goosashada, dhererka weelka qaboojinta, heerkulka biyaha, kala dheeraynta xadhigga, biyo-baxa iyo jiidista pelletizer waa inay u shaqeeyaan sidii hal nidaam.

Nanhaiya xogta khadka mataanaha ah ee hal iyo barbar socota

Qiimaha soo socdaa waxa ay ka yimaaddaan bogga wax soo saarka Nanhaiya. Waxay faa'iido u leeyihiin isbarbardhigga qaabeynta la daabacay. Qandaraaska wax iibsiga waa inuu ku celiyaa qiyamka ugu dambeeya ee walxaha la ansixiyay, kaaliyeyaasha iyo xaaladaha tijaabada.

Shayga Nanhaiya xariiqa pelletizing-ka-bilow Nanhaiya oo isbarbar socda khadka pelletizing mataanaha ah
Awoodda la daabacay 100 kg/h 300 ilaa 600 kg/h
Awoodda ugu weyn 75 kW motor ugu weyn 160 kW
Awood kuleyliyaha 120 kW Aan si gooni ah loo taxay
Nooca sharoobada Kaashashka kali ah Isbarbar yaaca mataanaha
Dhererka maroojinta iyo dhexroorka La habeeyay La habeeyay
Wax daabacan oo la daabacay 38CrMoAlA 38CrMoAlA
Kala duwanaanshaha walxaha la daabacay PVC, CaCO3 Masterbatch, TR, PET, PS, Eva, ABS, PE, TPR, TPE, TPV iyo PP PE, PP, PVC, ABS, HDPE, HDPE/PP, PA, PE/PP, LLDPE, ABS/PP iyo PPR
Qalabka khadka xudunta u ah Soo saarista, dhalaali sifaynta, madaxa dhinta, qaboojinta biyaha, pelletizer iyo ururinta Dhaqdhaqaaqa qulqulka sare, shaandhaynta dhalaalida, madaxa dhinta, pelletizer giraanta biyaha, qaboojinta iyo ururin otomaatig ah
Faahfaahinta alaabta Nitrided screw iyo foosto, pelletizer, haanta biyaha, shaashadda gariirta, silo iyo xakamaynta PLC Qalab adag oo adag iyo foosto, canaasiir modular ah, bamka dhalaalay, dhinta, giraanta biyaha ama pelletizer, saxan, shaashad gariir iyo silo
Ikhtiyaarada Beddel toos ah shaashadda, vacuum degesing iyo quudinta kaaliyaha Fakuum degeyska, beddelka shaashadda tooska ah, quudinta mataanaha ah ee buuxinta iyo la socodka fogaanta
Saamiga gearbox ee la daabacay Aan liiska ku jirin 2.5:1 ama 3:1
Taageero Rakibaadda fog, hawlgelinta iyo hagidda hawlgalka Tilmaamaha rakibidda, taageerada hawlgelinta iyo tababarka hawl-wadeennada
Modular twin-screw barrel sections arranged in the Nanhaiya workshop
Qaybaha foostada moodada ah waxay bixiyaan dekedo iyo aagagga hawsha. Habka ugu dambeeya waa inuu muujiyaa quudinta, hawo-qaadista, fuustooyinka xiran iyo isku xirka dheecaanka.
Nanhaiya vibrating screen for classifying finished plastic pellets
Baadhitaanka hoose waa qayb ka mid ah xakamaynta tayada pellet. Sheeg ganaaxyada la aqbali karo, cabbirka iyo habka ururinta.

Nanhaiya waxay xarunteedu tahay Zhoushan, Zhejiang, waxayna soo saartaa boolal, fuustooyin iyo qalab caag ah. Iibsadayaasha ayaa dib u eegi kara warshaddaqalabka wax soo saarka, shahaadooyinkaiyohabka adeeggadooda farsamada ka hor.

Isbarbardhigga u beddel qeexid iibsi

RFQ faa'iido leh ayaa ka dhigaysa xigashooyinka tartamaya mid is barbar dhig ah. Waxa kale oo ay ka hortagtaa in khadka lagu nashqadeeyo agagaarka muunad nadiif ah halka wax soo saarku uu hadhow helo quudinta qoyan, boodhka ama cufnaanta hoose.

  • Darajo kasta oo polymer ah iyo boqolkiiba miisaanka
  • Bikrad, warshad ka dib ama asal-macmiilka kadib
  • Pellet, budo, jajab, filim ama qaab agglomerate
  • Cufnaanta ugu yar iyo tan ugu badan
  • Qoyaanka, kacsanaanta, urta iyo xaalada dhaqida
  • Nooca wasakhaysan, cabbirka iyo boqolleyda la filayo
  • Buuxinta, midabka, fiber-ka iyo faahfaahinta wax lagu daro
  • Habka quudinta ee loo baahan yahay walxo kasta
  • Soo-saarka hadda iyo bartilmaameedka wax-soo-saarka saafiga ah ee la iibin karo
  • Daaqadda heerkulka dhalaalka ee la oggol yahay
  • Sifeynta shaandhaynta iyo qorshaha beddelka shaashadda
  • Dookhyada, giraanta biyaha ama biyaha hoostooda ee pelletizing
  • Cabbirka pellet, qaabka, qoyaanka iyo ganaaxyada xaddidan
  • Midabka loo baahan yahay, qulqulka dhalaalka ama tijaabooyinka farsamada
  • Danab la heli karo, inta jeer, biyo iyo hawo cadaadis leh
  • Qaabka dhirta, qolka madaxa iyo jihada agabka-socodka
  • Xakamaynta luqadda, diiwaan gelinta xogta iyo heerka badbaadada
  • Qaybaha taranka, hawlgelinta iyo baaxadda tababarka

Ha qorin "wax soo saarka: 500 kg/h" keligiis.Sheeg qaabaynta saxda ah, xaaladda quudinta, heerka diidmada la oggol yahay iyo muddada tijaabada. Dheecaannada guud ee ka-soo-baxa la midka ah lama mid aha kuwa qallalan, ee la baaray, ee la iibin karo ee la geeyo nidaamka ururinta.

Ilaalinta xidhashada sidoo kale waxay iska leedahay marxaladan. Buuxiyeyaasha abrasive, fiber galaaska iyo dib-u-warshadaynta wasakhaysan ayaa bedeli kara istaraatiijiyada birta iyo alaabta foosto. Dib u eeg Nanhaiyaqaybaha mataanaha ah ee isku midka ah, boolal haliyoqaybaha spareoo leh quudinta la filayo, halkii lagu dari lahaa doorasho guud oo adag dhamaadka.

Aqbal xariiqda agab iyo natiijooyin la qiyaasi karo

Tijaabada wareegta aan culayska saarnayn waxay hubisaa isu imaatinka, laakiin ma caddaynayso waxqabadka pelleting. Tijaabada aqbalaadda warshadu waa inay isticmaashaa walxo la isku raacay ama wax u dhigma oo si cad loo diiwaangeliyay waana inay socotaa wakhti dheer oo ku filan si ay u soo bandhigto quudinta, cadaadiska, hawo-qaadista iyo goynta xasilloonida.

  1. Xaqiiji walxaha tijaabadaRikoor badan, caanaha caanaha, qaabka quudinta, cufnaanta badan, qoyaanka iyo diyaarinta. Hayso muunad la hayo.
  2. Xaqiiji baaxadda khadka iyo badbaadada.Hubi matoorada, kuleyliyeyaasha, ilaaliyaha, qufulka, joogsiyada degdega ah, yutiilitida, qalabka iyo wareegtada ka hor quudinta polymerka.
  3. Gaadhi hawlgal joogto ah.Diiwangeli heerka quudiyaha, xawaaraha isbiirta, dejinta aagga, heerkulka dhalaalka ee la qiyaasay, cadaadiska, culayska socodka ama matoorka, faakuumka iyo xaaladaha qaboojinta.
  4. Cabir wax soo saarka la iibsan karo.Miisaanka pellets qalalan ka dib baaritaanka wakhti go'an. Diiwaangeli qashinka bilawga ah, jebinta xadhigga, agglomerates iyo isbeddellada shaashadda si gooni gooni ah.
  5. Tijaabi tayada pelletIsticmaal cabbirka pellet ee lagu heshiiyey, ganaaxyada, qoyaanka, cufnaanta bulk, midabka, qulqulka dhalaalka, kala firdhisanaanta ama tijaabooyinka qaabaynta.
  6. La tartamo dhacdo caadi ahMuuji beddelka shaashadda, dib u bilaabashada caadiga ah, soo kabashada quudiyaha ama isbeddelka midabka haddii ay muhiim tahay wax soo saarka maalinlaha ah.
  7. Kormeer mashiinka.Hubi hawo-qaadista, kaydka dhinta, xaalad goynta, qaylada aan caadiga ahayn, daadinta iyo meelaha nadiifinta ee la heli karo ka dib orodka.

Aragtida warshadeena:ha aqbalin xariiq sababtoo ah waxay si kooban u gaartaa wax soo saarka cinwaanka. Waxaan raadineynaa daaqad xasiloon: quudiyaha waa uu buuxsamaa, cadaadisku ma dhaqaaqo, dabaysha ayaa iska sii socota, gooyuhu ma abuuro ganaaxyo xad-dhaaf ah iyo pellets ayaa la kulma imtixaanka hoose ee iibsadaha. Wax-soo-saarka la iibin karo oo xasiloon ayaa ah tirada muhiimka ah.

Su'aalaha soo noqnoqda

Ma khadka pelletizing mataanaha ah ayaa had iyo jeer ka fiican xariiqda hal-dhalo?

Maya. Xariiqa isku midka ah ee mataanaha ah ayaa xoog badan marka habsocodku ay tahay in ay isku daraan polymers, kala firdhiyaan wax-buuxiyeyaasha ama midabada, ku dara maaddooyinka iyada oo loo marayo feederiyeyaasha dhinac, ama ka saara isbeddellada muhiimka ah. Xariiqda hal-xidhaale badanaa waa doorashada tooska ah marka xooluhu deggan yihiin, diyaarsan inta badan u baahan dhalaalid, shaandhayn, abuur cadaadis iyo goynta pellet.

Xariiqkee pelletizing ayaa u fiican PE ama PP dib loo warshadeeyay?

Waxay kuxirantahay xaalada regrind. PE ama durdur PP oo la kala soocay, la dhaqay oo macquul ah oo joogto ah ayaa laga yaabaa inay ku habboonaato xariiq hal-dhar ah oo leh quudinta saxda ah, nadiifinta iyo dhalaalidda sifaynta. Hababka isku dhafan, buuxinta buuxinta, ur ama ka saarista kacsan, iyo dalabka isku-dhafka ayaa caddayn kara xariiq mataano-kormeer ah oo barbar socda.

Xariiqkee ayaan u dooran karaa masterbatch ama xeryahooda aadka loo buuxiyey?

Ku billow qiimaynta xariiq mataano-sharoole ah oo isbarbar socda sababtoo ah curiyayaasha fur-fudud iyo aagagga quudinta ee goonida ah waxay siinayaan koontarool badan oo la isku darka qaybsan iyo kala firdhiso. Nooca buuxinta, rarista, cufnaanta bulk, xoqida iyo kala firdhinta loo baahan yahay ayaa wali go'aamisa quudiyaha, qaabaynta isku xidhka iyo xirmada xidhashada.

Xariiqa pelletizing-ka-bilow ma isticmaali karaa vacuum degesing?

Haa Nanhaiya waxay ku siinaysaa vacuum degesiga ikhtiyaar ahaan xariiqeeda pelletizing-ka-fure. Booska hawo-mareenka, heerka buuxinta maroojinta, qoyaan quudinta, dhalaalidda shaabadda iyo awoodda faakuumka waa inay wada shaqeeyaan si aanay alaabtu u daadin hawo-mareenka.

Waa maxay faraqa u dhexeeya xadhig iyo giraanta biyaha?

Nidaamka xargaha ayaa soo saara xadhig joogto ah, qaboojiya ka dibna u gooyaa pellets cylindrical ah. Nidaamka giraanta biyuhu wuxuu gooyaa dhalaalka wejiga dhinta wuxuuna ku qaadaa pellet-ka biyaha. Dabeecadda maaddooyinka, wax-soo-saarka, baahiyaha beddelka, qaabka pellet iyo ka-qaybgalka hawlwadeenku waa inay go'aamiyaan habka.

Intee in le'eg ayay soo saari karaan khadadka pelletizing Nanhaiya?

Nanhaiya waxay taxday 100kg/saacadiiba xariiqa xadhkaha goosha leh iyo 300 ilaa 600 kg/h Kuwani waa habaynta alaabta la daabacay, markaa xigashada kama dambaysta ahi waa inay sheegtaa qaabaynta saxda ah, xaaladda quudinta iyo saldhigga aqbalaadda mashiinka la doortay.

Macluumaad noocee ah ayaan ku soo diri karaa khadka pelletizing RFQ?

U dir darajooyinka polymerka iyo boqolleyda, foomka quudinta, cufnaanta bulk, qoyaanka, wasakhda iyo heerarka kacsan, wax lagu daro iyo buuxinayaasha, soosaarka xaadirka ah iyo kuwa bartilmaameedka ah, cabbirka pellet, shuruudaha sifaynta, xaaladaha tamarta, qaabka dhirta, heerka xakamaynta iyo tijaabada aqbalida la qiyaasi karo.

Shaacinta ganacsiga: Nanhaiya waxay soo saartaa xadhkaha pelletizing, boolal, fuustooyin iyo qaybaha wax-soo-saarka ee ku xidhan hagahan. Xulashada kama dambaysta ahi waxay ku xidhan tahay alaabta iibsadaha, baaxadda khadka la ansixiyey, heshiiska farsamada iyo tijaabada aqbalaadda.

Wararka la xidhiidha
Fariin ii dhaaf
X
Waxaan isticmaalnaa cookies si aan kuu siino khibrad wax barasho oo wanaagsan, u falanqeyso taraafikada goobta iyo shaqsiyeynta macluumaadka. Isticmaalka boggan, waxaad ogolaatay isticmaalkayada cookies-ka. Siyaasadda Qarsoonnimada
DiidAqbal